Steel alloys susceptible to case and core hardening comprising 0.05 to 0.24 weight percent carbon; 15 to 28 weight percent cobalt and 1.5 to 9.5 weight percent in nickel, small percentages of one or more additives: chromium, molybdenum, and vanadium; and the balance iron.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 15.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A class of steel alloys comprising, in combination: a case hardened mixture with a core composition of about 0.05 to about 0.25 weight percent carbon in combination with about 15 to 28 weight percent cobalt, about 1.5 to 9.5 weight percent nickel, and one or more additives selected from the group consisting of about 3.5 to 9 weight percent chromium, less than about 2.5 weight percent molybdenum, and less than about 0.2 weight percent vanadium and the balance iron, where the mixture is case hardened in the range of surface hardness greater than about 60 Rockwell C and wherein the case layer is
- Claim 2Independent Claim
A class of steel alloys comprising, in combination: a case hardened mixture with a core composition of about 0.5 to about 0.25 weight percent carbon in combination with about 15
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (6)
Non-Patent Literature (1)
- English abstract of European patent 269603B, Rotter et al, published Jun. 1988.