Abstract
A green compact of a rare earth alloy magnetic powder is made by pressing the powder. The powder is pressed within an air environment that has a temperature controlled at 30° C. or less and a relative humidity controlled at 65% or less.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 15.
Claims (3 — 3 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming a green compact of a rare earth alloy magnetic powder comprising the steps of: providing a rare earth alloy powder, providing a controlled environment having a temperature ranging from 5° C. to 30° C. and a relative humidity ranging from 40% to 65%, and pressing the rare earth alloy powder within the controlled environment.
- Claim 2Independent Claim
A method of forming a green compact of a rare earth alloy magnetic powder comprising the steps of: providing a rare earth alloy powder, providing a controlled environment having a temperature ranging from 5° C. to 30° C. and a relative humidity ranging from 40% to 65% and a dew point of at least 6° C. less than the temperature, and pressing the rare earth alloy powder within the controlled environment.
- Claim 3Independent Claim
The method of claim
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (2)
- Inventors: Seiichi Kohara et al., U.S. patent application Ser. No. 09/421,237, filed: Oct. 20, 1999, Specification and Drwaings, Title: "Powder Pressing Apparatus and Powder Pressing Method".
- Inventors: Seiichi Kohara et al., U.S. patent application Ser. No. 09/472,247 and Amendment, filed: Dec. 27, 1999, Specification and Drawings, Title: Process and Apparatus for Supplying Rare Earth Metal-Based Alloy Powder.