Method for forming a gate for semiconductor devices

4Forward Citations (#26090608 Global)
0.2/yrCitation Velocity (#36314499 Global)
1.24Citation PageRank (#30612856 Global)
4Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention discloses a method for forming a gate for semiconductor devices by depositing a TaO x N y film as a gate oxide film. The method includes the steps of providing a semiconductor substrate where a device isolation film has been formed, growing an SiO 2 or SiON film on the semiconductor substrate, depositing an amorphous TaO x N y film on the SiO 2 or SiON film, performing a low temperature annealing process to improve quality of the amorphous TaO x N y film, performing a high temperature annealing process ex-situ to remove organic substances and nitrogen in the amorphous TaO x N y film, and crystallize the amorphous TaO x N y film, and depositing a metal barrier film on the crystallized TaO x N y film, and depositing a polysilicon film or metal film for a gate electrode on the metal barrier film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for forming a gate for semiconductor devices, comprising the steps of: providing a semiconductor substrate; forming one of a SiO 2 film and a SiON film on the semiconductor substrate; forming an amorphous TaO x N y film on the one of the SiO 2 and SiON films; performing a low temperature annealing process on the amorphous TaO x N y film; crystallizing the amorphous TaO x N y film by performing a high temperature annealing process; and forming one of a polysilicon film and a metal film on the crystallized TaO x N y film.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the one of the SiO 2 film and the SiON film is formed by performing a rapid thermal process at a temperature between about 700° C. and 1100° C. in an atmosphere of one of O 2 gas and N 2 O gas.