Patents
US 6,441,129 B2#10785790 Most CitedExpiredUnited States (USPTO)Utility

High temperature solid state polymerization of poly (trimethylene terephthalate)

10Forward Citations (#10785790 Global)
0.4/yrCitation Velocity (#19297063 Global)
1.66Citation PageRank (#19506106 Global)
17Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention is a process for producing poly(trimethylene terephthalate) (PTT) at an increased solid state polymerization rate, wherein 1,3-propane diol and an aromatic acid or a dialkyl ester thereof are esterified or transesterified, the esterification or transesterification product is polycondensed, and the polycondensation product is pelletized and then subjected to continuous solid state polymerization at a temperature of 200 to 225° C., preferably 210 to 225° C. In one embodiment of the present invention, the temperature range is 200 to 220° C., and the pellet size of the polymer to be solid state polymerized is from 1.0 to 1.5 g/100. In another embodiment of the present invention, the solid state polymerization is carried out at 210 to 225° C. for from 1 to 20 hours and then the temperature is increased to above the initial melting point of the polymer to produce a PTT polymer with an intrinsic viscosity of 1.3 dl/g or greater.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 10.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for producing poly(trimethylene terephthalate) and achieving an increased solid state polymerization rate wherein 1,3-propanediol, and optionally other diols, and an aromatic acid or diester thereof are esterified or transesterified, the esterification or transesterification product is polycondensed to produce a prepolymer, and the prepolymer is subjected to continuous solid state polymerization at a temperature of 210 to 225° C. and then at a temperature above the normal melting point of the prepolymer for 1 to 20 hours to produce a polymer with an intrinsic viscosity of 1.3 d/g or

  2. Claim 2Depends on #1

    The process of claim 1 wherein the prepolymer is polymerized at 210 to 225° C. for 1 to 10 hours and then polymerized above the normal melting point of the prepolymer f

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • "PET SSP: One of the Key Steps in PET Manufacturing," Paper presented in Buhler Pro Tech Forum '96, Uzwil, Switzerland, Jun. 20-21, 1996.