Method for the formation of a thin optical crystal layer overlying a low dielectric constant substrate
Abstract
A method for the formation of a thin optical crystal layer (e.g., a thin LiNbO 3 optical single crystal layer) overlying a low dielectric constant substrate (e.g., a low dielectric constant glass substrate). The method includes implanting ions (e.g., He + ) through a surface of an optical crystal substrate. The implanting of the ions defines, in the optical crystal substrate, a thin ion-implanted optical crystal layer overlying a bulk optical crystal substrate. A low dielectric constant substrate is subsequently bonded to the surface, using either a direct or an indirect bonding technique, to form a bonded structure. The bonded structure is thermally annealed at a temperature in the range of 300° C. to 600° C. for 30 minutes to 300 minutes. Thereafter, the thin ion-implanted optical crystal layer and low dielectric constant substrate are separated from the bulk optical crystal substrate using mechanical force applied to the low dielectric constant substrate and/or the bulk optical crystal substrate in the direction of separation. As a result, a thin optical crystal layer overlying a low dielectric constant substrate is formed. The thin optical crystal layer has characteristics (e.g
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for the formation of a thin optical crystal layer overlying a low dielectric constant substrate comprising: implanting ions into an optical crystal substrate, thereby defining therein, a thin ion-implanted optical crystal layer overlying a bulk optical crystal substrate; bonding a low dielectric constant substrate to the ion-implanted optical crystal layer to form a bonded structure; thermally annealing the bonded structure at a temperature in the range of 300° C. to 600° C. for 30 minutes to 300 minutes; and separating the thin ion-implanted optical crystal layer and low dielectric c
Technical Overview & Description