Manufacturing method for organic EL device
Abstract
A method for manufacturing an organic EL display device is provided, capable of improving an opening ratio and providing narrower pitches for narrowing non-lighting portion between pixels, and, at the same time, capable of eliminating short-circuiting between display pixels for eliminating cross-talk and non-lighting pixels. In the deposition process of the cathode 6 , the incident angle of the deposition material onto the substrate is optimized by optionally changing parameters such as a distance between the substrate 1 and the mask 11 and a distance between the substrate and the point deposition source 13 . Thus, deposition material from a plurality of deposition sources impinges onto the substrate surface obliquely passing at a different incident angles though opening (slits 11 a ) of the mask 11 , so that the width 10 of the electrode pattern 6 becomes broader than the width of the slit by superposition of the deposition material passing through the slits at different incident angles.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 42.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An organic EL display device manufacturing method comprising: forming a first stripe-shaped electrode pattern on a substrate surface; forming a plurality of layers including an organic layer on the substrate surface including said first electrode pattern; and forming a second stripe-shaped electrode pattern on said first electrode pattern in the orthogonal direction to said first electrode pattern by disposing a mask between a plurality of deposition sources of the electrode material and the substrate separated at a predetermined distance from said substrate and by supplying a deposition mater
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗