Reduced shrinkage in metallocene isotactic polypropylene fibers
Abstract
The present invention relates to a method for the production of polypropylene fibers resulting in improved shrinkage percentages and to polypropylene fibers themselves having improved shrinkage percentages. The method includes providing a polypropylene polymer with a melt flow index of no more than about 25 grams per 10 minutes. This polymer should include isotactic polypropylene produced by the polymerization of propylene in the presence of an isospecific metallocene catalyst. The polymer is then heated to a molten state and extruded to form a fiber preform. The preform is spun and subsequently drawn at a take-away speed and a drawing speed providing a draw ratio of no more than about 3, and more preferably no more than about 2.5, to produce a continuous polypropylene fiber. The fiber based on metallocene catalyzed isotactic polypropylene demonstrates improved shrinkage properties of at least about 10% and at some draw ratios at least about 25% over the shrinkage properties of Ziegler-Natta catalyzed isotactic polypropylenes having similar melt-flow indices. In the same method, when the polymer is heated to a molten state, the polymer is preferably heated in a feeding zone to a te
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 17.
Claims (3 — 3 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for the production of polypropylene fibers, comprising a) providing a polypropylene polymer with a melt flow index of no more than about 25 grams per 10 minutes, comprising isotactic polypropylene produced by the polymerization of propylene in the presence of an isospecific metallocene catalyst; b) heating said polypropylene polymer to a molten state and extruding said molten polymer to form a fiber preform; and c) spinning said fiber preform and subsequently drawing said preform at a take-away speed and a drawing speed providing a draw ratio of no more than about 3 to produce a conti
- Claim 2Independent Claim
The method of claim I wherein said fiber is formed with a take-away speed and a drawing speed providing a draw ratio of no more than about 2.5.
- Claim 3Independent Claim
The method of claim
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (19)
Non-Patent Literature (1)
- US 5,242,876, 09/1993, Shamshoum et al. (withdrawn)