US 6,399,686 B1#33399778 Most CitedExpiredUnited States (USPTO)Utility

Anti-reflective coating compositions comprising polymerized aminoplasts

3Forward Citations (#33399778 Global)
0.1/yrCitation Velocity (#41571594 Global)
1.04Citation PageRank (#39528028 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Improved anti-reflective coating compositions for use in integrated circuit manufacturing processes and methods of forming these compositions are provided. Broadly, the compositions are formed by heating a solution comprising a compound including specific compounds (e.g., alkoxy alkyl melamines, alkoxy alkyl benzoguanamines) under acidic conditions so as to polymerize the compounds and form polymers having an average molecular weight of at least about 1,000 Daltons. The monomers of the resulting polymers are joined to one another via linkage groups (e.g., —CH 2 —,—CH 2 —O—CH 2 —) which are bonded to nitrogen atoms on the respective monomers. The polymerized compound is mixed with a solvent and applied to a substrate surface after which it is baked to form an anti-reflective layer. The resulting layer has high k values and can be formulated for both conformal and planar applications.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a polymer composition, said method comprising the steps of: providing a dispersion including a quantity of a compound according to the formula: wherein each X is individually selected from the group consisting of NR 2 and phenyl groups, where each R is individually selected from the group consisting of hydrogen, alkoxyalkyl groups, carboxyl groups, and hydroxymethyl groups; adding to said dispersion from about 0.001-1 moles of an acid per liter of said dispersion; and heating said dispersion to a temperature of at least about 70° C. for at least about 2 hours to yield th

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said acid addition step comprises adding p-toluenesulfonic acid to said dispersion.

  3. Claim 3Depends on #1

    The method of claim 1