Method for forming resist pattern
Abstract
A method for forming a resist pattern includes the steps of: forming an underlayer transparent film on a semiconductor substrate; forming a resist film on the transparent film to a thickness set to be m·λ/2n 2 , where λ is an exposure wavelength, n 2 is a refractive index of the resist film, and m is an integer from 5 to 30; applying a water-soluble antireflection film on the resist film to a thickness set to be λ/4n 1 , where n 1 is a refractive index of the antireflection film; and exposing the resist film from above the antireflection film by a beam having a wavelength λ and developing the resist film as well as removing the antireflection film.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 15.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for forming a resist pattern with a high dimension of controllability, the method comprising: forming an underlayer transparent film on a semiconductor substrate; forming a resist film on the underlayer transparent film to a thickness set to be m·λ/2n 2 , where λ is an exposure wavelength, n 2 is a refractive index of the resist film, and m is an integer from 5 to 30; applying a water-soluble antireflection film on the resist film to a thickness set to be λ/4n 1 , where n 1 is a refractive index of the water-soluble antireflection film; and exposing the resist film from above the wa
- Claim 2Depends on #1
The method of claim 1 , wherein the beam having a wave
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗