Patents
US 6,387,516 B2#2694620 Most CitedExpiredUnited States (USPTO)Utility

Interlayer for laminated glass and laminated glass

27Forward Citations (#2694620 Global)
1.1/yrCitation Velocity (#5567660 Global)
4.03Citation PageRank (#4711047 Global)
7Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention has it for its object to provide an interlayer film for laminated glass and a laminated glass which shows a much decreased extent of blushing of the peripheral region thereof even when placed in a high-humidity atmosphere, without compromise in those fundamental performance characteristics which are required of laminated glass, such as transparency, weather resistance, adhesion and penetration resistance. The present invention is related to an interlayer film for laminated glass comprising a plasticized poly(vinyl acetal) resin and having the haze after 24 hours of immersion is not more than 50% when said interlayer film with a thickness of 0.3 to 0.8 mm is immersed in water at 23° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 27.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An interlayer film for laminated glass comprising a plasticized poly(vinyl acetal) resin and a sodium salt wherein the sodium salt in said interlayer film has a particle diameter of not greater than 5 μm and said interlayer having the haze after 24 hours of immersion of not more than 50% when said interlayer film with a thickness of 0.3 to 0.8 mm is immersed in water at 23° C.

  2. Claim 2Depends on #1

    The interlayer film for laminated glass according to claim 1 wherein the concentration of sodium in the interlayer film is not greater than 50 ppm.

  3. Claim 3Independent Claim

    An interlayer film for laminated glass comprising a plasticized poly(vinyl acetal) resin and a potassium salt wherein the particle diameter of the potassium salt in the interlayer film is not greater than 5 μm and said interlayer having the haze after 24 hours of immersion of not more

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Patent Abstracts of Japan, vol. 15, No. 115, Mar. 19, 1991 & JP 03 005772 A, Jan. 11, 1991.