Process for producing hard, electrodeposited iron with inherent channel porosity
Abstract
A process of producing an iron plating on a metal surface of a part is provided. The process includes the steps of forming and maintaining an electrolytic plating bath to comprise: 200-500 Gm/L ferrous sulfate; 20-70 Gm/L ferrous fluoborate; 10-35 Gm/L ammonium chloride; and an effective amount of wetting agent in an aqueous solution; maintaining the pH of the bath in the range of 1.5 to 4.2; maintaining the temperature of the bath in the range of 100° F. to 160° F.; and maintaining the current density in the bath in the range of 2 to 60 amps/sq.ft. At least the metal surface of the part to be plated is contacted with the electrolytic plating bath. According to a further aspect of the invention, during electroplating, the pH, the temperature, and/or the current density are changed within their specified ranges to control the microstructure of the electrodeposited iron. An iron plating on a part can be produced wherein the iron plating has a surface network of channel type porosity wherein the channels are in the range of 0.0005 inch to less than 0.010 inch deep, and wherein the iron plating has a preplate strata having a hardness ranging from 35 to 55 Rc.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process of producing an iron plating on a metal surface of a part comprising the steps of: (a) forming and maintaining an electrolytic plating bath to comprise: 200-500 Gm/L ferrous sulfate; 20-70 Gm/L ferrous fluoborate; 10-35 Gm/L ammonium chloride; and an effective amount of wetting agent in an aqueous solution; (b) maintaining the pH of the bath in the range of 1.5 to 4.2; (c) maintaining the temperature of the bath in the range of 100° F. to 160° F.; (d) maintaining the current density in the bath in the range of 2 to 60 amps/sq. ft.; (e) contacting the metal surface of the part to be p
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 6,589,412 B1 | Method for producing a sliding member having excellent seizure resistance | 2003 | 9 |
References Cited — Backward Prior Art (9)
Non-Patent Literature (1)
- Product Brochure-Iron Plating, Metal Finishing Guidebook and Directory Issue, vol. 93, No. 1A, pp. 255-258, 1995, reprinted in same publication in 1996, 1997, and 1998. No month available.