Aluminum alloy support for lithographic printing plate and process for producing substrate for support
Abstract
The present invention provides a support for a lithographic printing plate prepared by cold rolling a sheet while intermediate annealing is omitted to save energy and the number of the cold rolling steps are decreased to simplify the sheet production steps and to give a desired strength of the sheet, and by inhibiting precipitation of Si particles in the substrate to give extremely excellent resistance to ink staining in the nonimage areas during printing, and a process for producing a substrate therefore. The production process comprises homogenization heat-treating an aluminum alloy slab comprising 0.10 to 0.40 wt % of Fe, 0.03 to 0.15 wt % of Si, 0.004 to 0.03 wt % of Cu, and the balance of Al and unavoidable impurities, hot rolling the heat-treated slab, and cold-rolling the hot-rolled strip without intermediate annealing, the cold rolling including a final pass after which the sheet temperature becomes at least the recovery temperature of the sheet and the following rapid cooling, whereby an aluminum alloy substrate for a lithographic printing plate having a content of precipitated Si of up to 30 ppm and a tensile strength of from 145 to 180 MPa is produced. When the aluminum
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An aluminum alloy support containing precipitated Si for a lithographic printing plate prepared by homogenization heat-treating an aluminum alloy cast slab, hot rolling the slab to form a hot rolled strip, cold rolling the hot roiled skip without intermediate annealing to form a substrate, graining the substrate, and anodically oxidizing the substrate, said substrate comprising 0.10 to 0.40% of Fe, 0.03 to 0.15% of Si, 0.004 to 0.03% of Cu, and the balance of Al and unavoidable impurities including precipitated Si in an amount no more than 30 ppm, an anodic oxide film from 0.1 to 1.0 μm thick
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗