High rate silicon deposition method at low pressures
Abstract
A method for high rate silicon deposition at low pressures, including a method of operating a CVD reactor having a high degree of temperature and gas flow uniformity, the method of operation providing a novel combination of wafer temperature, gas flow and chamber pressure. According to the method, a substrate is placed in a vacuum chamber wherein a reactant gas is provided at a high velocity in parallel with the substrate via a plurality of temperature controlled gas injectors providing a condition wherein the deposition rate is only limited by the rate of delivery of unreacted gas to the substrate surface and the rate of removal of reaction byproducts. The novel combination of process conditions moves the reaction at the wafer surface into the regime where the deposition rate exceeds the crystallization rate, resulting in very small crystal growth and therefore a very smooth polysilicon film with a surface roughness on the order of 5-7 nm for films 2500 angstroms thick. The process is configured to operate below what is known as the “transition” temperature, at which level each layer of film is deposited in an amorphous form and then crystallizes as the deposition proceeds because
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 21.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of depositing silicon, comprising: depositing silicon on a wafer including the steps of (a) placing a wafer on a carrier in a deposition chamber; (b) rotating said carrier about a central axis of said carrier for equalizing distribution of a process gas over said wafer; (c) heating said wafer to a temperature of at least 500° C. but below a transition temperature below which a deposition rate of silicon exceeds a crystallization rate; (d) injecting said process gas substantially parallel to a surface of said wafer at a velocity of at least 10 cm/sec with a pressure in said deposition
- Claim 2Depends on #1
A method as recited in claim 1 wherein said wafer is heated to a temperature between 500° C. and 700° C.
- Claim 3Depends on #1
A method as recited in claim 1 whe
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 21 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,976,996 A | Chemical vapor deposition reactor and method of use thereof | 1990 | 213 |
| US 5,551,985 A | Method and apparatus for cold wall chemical vapor deposition | 1996 | 110 |
Non-Patent Literature (1)
- Pierson, Handbook of Chemical Vapor Deposition, Noyes Publications, Park Ridge, New Jersey, USA, (1992), pp. 184-185 (no month).