Yarn formed of eastane fibers produced by the dry spinning or wet spinning of spinning solutions which include polydimethylsiloxane and ethoxylated polydimethylsiloxane
Abstract
The invention relates to a spinning process, more particularly a dry spinning process, for the production of elastane fibers in which 0.8 to 2% by weight of polydimethylsiloxane with a viscosity of 50 to 300 cSt and 0.2 to 0.6% by weight of ethoxylated polydimethylsiloxane with a viscosity of 20 to 150 cSt are added to the elastane spinning solution before it is spun.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A yarn formed of elastane fibers produced from polyurea polyurethane by dry spinning or wet spinning to form filaments, removing the spinning solvent, finishing, optionally twisting to form filaments, and winding the spun filaments, wherein A) from 0.8 to 2% by weight of polydimethylsiloxane having a viscosity of 50 to 300 cSt and B) from 0.2 to 0.6% by weight of ethoxylated polydimethylsiloxane having a viscosity of 20 to 150 cSt (Viscosities measured with a falling ball viscosimeter at 25° C.) the percentages being based on the siloxane content of the final fiber, are added to the spinning s
- Claim 2Depends on #1
The yarn of claim 1 , wherein the polyurea polyurethane solution is dry spun.
- Claim 3Depends on #1
The yarn of claim 1 , wherein the weight ratio of A:B is 1:1 to 5:1.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (1)
- G. Oeutel, Polyurethane Handbook, 2Edition, Hauser Publishers, 1993, pp. 630-643.