Patents
US 6,222,000 B1#5310189 Most CitedExpiredUnited States (USPTO)Utility

Process for producing amorphous anisotropic melt-forming polymers having a high degree of stretchability

17Forward Citations (#5310189 Global)
0.7/yrCitation Velocity (#11173164 Global)
3.05Citation PageRank (#7378373 Global)
27Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Process for producing highly stretchable, amorphous anisotropic melt-forming polymers having recurring units derived from p-hydroxybenzoic acid, 6-hydroxy-2-naphthoic acid, at least one aromatic diacid and at least one aromatic diol and/or hydroxyamine component, at least a portion of which is 4,4′-biphenol, which process comprises incorporating into such polymers recurring units derived from one or more aromatic monomers that provide the polymers with selected meta-linkages wherein each of said recurring units is present in the polymer in specific amounts.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 17.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for forming highly stretchable, amorphous anisotropic melt-forming polymers which comprises incorporating recurring unit V selected from the group consisting of: and mixtures thereof, wherein R 1 is independently selected from the group consisting of hydrogen and C 1 to C 6 alkyl, into a polymer comprising recurring units I, II, III, and IV, wherein recurring unit I is recurring unit II is: recurring unit III is: wherein Ar 1 is selected from the group consisting of: and mixtures thereof; and recurring unit IV is: —O—Ar 2 —X—  IV wherein Ar 2 is selected from the group consistin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (27)

PatentTitleYearCitations
US 4,351,918 APoly(ester-amide) capable of forming an anisotropic melt phase derived from 6-hydroxy-2-naphthoic acid, other aromatic hydroxyacid, carbocyclic dicarboxylic acid, and aromatic monomer capable of forming an amide linkage198296
US 4,473,682 AMelt processable polyester capable of forming an anisotropic melt comprising a relatively low concentration of 6-oxy-2-naphthoyl moiety, 4-oxybenzoyl moiety, 4,4'-dioxybiphenyl moiety, and terephthaloyl moiety1984115
US 4,522,974 AMelt processable polyester capable of forming an anisotropic melt comprising a relatively low concentration of 6-oxy-2-naphthoyl moiety-4-benzoyl moiety, 1,4-dioxyphenylene moiety, isophthaloyl moiety and terephthaloyl moiety1985110
US 4,563,308 ARecovery of caprolactam from caprolactam-containing distillation residue198615
US 4,684,712 AProcess for producing wholly aromatic polyesters198741
US 4,722,993 AWholly aromatic mesomorphic polyester amides and the preparation thereof198813
US 4,918,154 APolyester resin exhibiting optical anisotropy in molten state and composition thereof199011
US 4,920,197 APolyester resin exhibiting optical anisotropy in molten state which contains a low concentration of 6-oxy-2-naphthoyl units and composition thereof19908
US 4,937,310 APolyester resin exhibiting optical anisotropy in molten state and composition thereof199013
US 4,966,956 AAromatic thermotropic copolyesteramide199018
US 4,983,713 APolyester resin exhibiting optical anisotropy in molten state containing minor amounts of 6-oxy-2-naphthoyl units199129
US 5,025,082 AAromatic polyester, aromatic polyester-amide and processes for producing the same199130
US 5,037,939 AThermotropic, fully aromatic polyesters prepared by polycondensation of aromatic diphenols and aromatic carboxylic acids199115
US 5,055,546 AProcess for producing aromatic polyesters199110
US 5,066,767 AWholly aromatic polyesters comprising isophthalic acid, terephthalic acid, p-hydroxybenzoic acid, hydroquinone and an arylene diol199114

Non-Patent Literature (4)

  • Anisotropic Polymers, Their Synthesis and Properties, G. W. Calundann and M. Jaffe, pp 247-291, Proceedings of the Robert A. Welch Conferences on Chemical Research XXVI, Synthetic Polymers, 1982.
  • D. S. Nagvekar et al, "New Wholly-Aromatic Thermotropic Polyesters with Controlled Flexibility", Materials Research Symposium Paper, Spring 1999.
  • R.S. Irwin, "Chain Folding in Thermotropic Polyesters", Macromolecules 1993, vol. 26, pp. 7125-7133.
  • W. J. Jackson, Jr., "Liquid Crystalline Aromatic Polyesters: An Overview", Journal of Applied Polymer Science: Applied Polymer Symposium, vol. 41, pp. 25-33 (1985).