Method of fabricating ferroelectric integrated circuit using dry and wet etching
Abstract
In a ferroelectric integrated circuit, a hydrogen barrier layer comprising titanium or titanium nitride or both is formed over a metal oxide element to protect it from hydrogen degradation. After hydrogen annealing and other process steps causing hydrogenating or reducing conditions, the hydrogen barrier layer is removed in a two-step etching process. The first etch step is a dry etch, preferably a standard ion-mill etching process, which rapidly removes most of the hydrogen barrier layer. The second step is a wet, chemical etch, preferably using a solution containing NH4OH, H2O2, and H2O, which selectively removes remnants of the hydrogen barrier layer from the circuit by oxidizing a chemical element of the barrier layer. The metal oxide material preferably comprises a layered superlattice compound.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 14.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for fabricating ferroelectric integrated circuits comprising the steps of: providing a substrate; forming on said substrate a thin film of a ferroelectric metal oxide material; forming a hydrogen barrier layer directly over at least a portion of said thin film of metal oxide material; performing a dry etch to remove a significant portion of said hydrogen barrier layer; and performing a wet, chemical etch to remove remnants of said hydrogen barrier layer, said etch being stopped on a material selected from the group consisting of conductors and a ferroelectric material.
- Claim 2Depends on #1
A method according to claim 1 wherein said dry etch is an ion-mill etching process.
- Claim 3Depends on #1
A method according to claim 1 wherein said wet etch comprises using a solution containing NH 4 OH, H 2 O 2 ,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (15)
Non-Patent Literature (4)
- Article: H. Achard and H. Mace; "Integration of Ferroelectric Thin Films For Memory Applications"; Science and Technology of Electroceramic Thin Films; Kluwer Academic Publishers, 1995; pp. 353-372, inclusive.
- Symposium Abstract: Ilsub Chung, et al.; "Integration of Ferroelectric Capacitors Using Multilayered Electrode"; The Tenth International Symposium on the Applications of Ferroelectrics, Aug. 18-21, 1996, Hilton Hotel, East Brunswick, NJ, Rutgers University; p. 55.
- Symposium Abstract: Takashi Hase, et al.; "Analysis of the Degradation of PZT and SrBi2Ta2O9 Thin Films With A Reductive Process"; The Eighth International Symposium on Integrated Ferroelectrics, Mar. 18-20, 1996, Tempe, AZ; Plenary Talks, Invited Lectures and Contributed Papers.
- Wolf et al., Silicon Processing for the VLSI Era: vol. 1, 1986, TK 7874 .W6 v. 1c.123, pp. 540-541.*