Patents
US 6,204,083 B1#6365306 Most CitedExpiredUnited States (USPTO)Utility

Process for producing infrared emitting device and infrared emitting device produced by the process

15Forward Citations (#6365306 Global)
0.6/yrCitation Velocity (#13010210 Global)
2.50Citation PageRank (#10151482 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In order, to manufacture a high-performance infrared-emitting element having high-speed thermal response characteristics and a high infrared emissivity, a bridge (heat-generating) portion having a separation space is formed on a silicon element substrate. The bridge portion is formed to have a thickness of 5 μm or less by doping boron as an impurity by ion implantation with a concentration distribution peak value of 1.5×10 19 atoms/cm 3 or more, and performing annealing under predetermined conditions for activating the impurity layer. In the infrared-emitting element manufactured in this manner, even if the bridge portion is made thin to improve the thermal response characteristics, the infrared emissivity does not decrease because of a high impurity concentration, and a large temperature modulation width can be obtained. In doping boron as the impurity by ion implantation, the dose is preferably set to 3.0×10 14 ions/cm 2 or more. To activate the impurity layer upon doping boron, the annealing is performed in the nitrogen gas atmosphere at a temperature of 1,100° C. to 1,200° C. for 5 min to 40 min and further in the wet oxygen atmosphere for about 25 min to 40 min. As a result, t

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 15.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An infrared-emitting element manufacturing method comprising: preparing a single-crystal silicon substrate serving as an element substrate; forming an impurity layer as a heavily doped region by doping boron from an upper surface side of said element substrate by ion implantation at a peak concentration of not less than 1.5×10 19 atoms/cm 3 in order to form a heat-generating portion having a predetermined shape on said element substrate; performing annealing for said element substrate having said impurity layer under a predetermined condition for activating said impurity layer; forming a pai

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Infrared Reflectivity And Transmissivity Of Boron-Implanted, Laser-Annealed Silicon, Herbert Engstrom, J. Appl. Phys., pp. 5245-5249, 51 (10), Oct., 1980.
  • Microheater Made Of Heavily Boron Doped Single Crystal Silicon Beam, Kimura et al, Technical Digest of the 11th Sensor Symposium, 1992, pp. 169-172.