Metal-resis bond grindstone and method for manufacturing the same
Abstract
The method disclosed here comprises the steps of (a) mixing metal powder, a resin, abrasive grains, and a solid reducing agent at the normal (room) temperature through the melting point of the reducing agent to form a mixture and (b) molding and baking the mixture at the melting point of the reducing agent through that of the metal powder. The solid reducing agent is a fatty acid, preferably stearic acid having a volume ratio of 5 to 20% with respect to the metal powder. With is, it is possible to make metal-resin bond grindstones that give such high-quality mirror surfaces that have conductivity fit for ELID grinding and are not liable to have chippings or scratches and also have an Rmax value of approximately 3 nm or less.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 3.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A metal-resin bond conductive grindstones, comprising: metal powder, a resin, abrasive grains, and a solid reducing agent which reduces said metal powder.
- Claim 2Independent Claim
A method for manufacturing a metal-resin bond grindstone, comprising the steps of: (a) mixing metal powder, a resin, abrasive grains, and a solid reducing agent at a temperature between about room temperature and a melting point of said reducing agent to form a mixture; and (b) molding and baking said mixture at a temperature between the melting point of said reducing agent and a melting point of said metal powder.
- Claim 3Depends on #2
The method of manufacturing a metal-resin bond grindstone according to claim 2 , wherein said solid reducing agent is a fatty acid.