Borophosphosilicate glass incorporated with fluorine for low thermal budget gap fill
Abstract
A method of depositing a fluorinated borophosphosilicate glass (FBPSG) on a semiconductor device as either a final or interlayer dielectric film. Gaps having aspect ratios greater than 6:1 are filled with a substantially void-free FBPSG film at a temperature of about 480 DEG C. at sub-atmospheric pressures of about 200 Torr. Preferably, gaseous reactants used in the method comprise TEOS, FTES, TEPO and TEB with an ozone/oxygen mixture. Dopant concentrations of boron and phosphorus are sufficiently low such that surface crystallite defects and hygroscopicity are avoided. The as-deposited films at lower aspect ratio gaps are substantially void-free such that subsequent anneal of the film is not required. Films deposited into higher aspect ratio gaps are annealed at or below about 750 DEG C., well within the thermal budget for most DRAM, logic and merged logic-DRAM chips. The resultant FBPSG layer contains less than or equal to about 5.0 wt % boron, less than about 4.0 wt % phosphorus, and about 0.1 to 2.0 wt % fluorine.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 16.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming a fluorine doped oxide glass film on a semiconductor device in a chemical vapor deposition chamber comprising the steps of: (a) providing a semiconductor device in said chamber; (b) providing a gaseous silicon source; (c) providing a gaseous oxygen source; (d) providing a gaseous fluorine source; (e) providing a gaseous boron source; (f) providing a gaseous phosphorus source; (g) injecting said gaseous sources into said chamber; and (h) depositing a layer of fluorine doped oxide glass on said semiconductor device at a temperature of about 480° C. to 650° C. an
- Claim 2Depends on #1
The method of claim 1, further including the step of reflowing said layer of doped oxide glass on said semiconductor substrate at a temperature o
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 16 total)
References Cited — Backward Prior Art (16)
Non-Patent Literature (1)
- J. Sato et al. Very Low Temperature CVD Of SIO 2 Films Using Ozone And Organosilane I.c.s Spring Meeting, May 1971, abstract No. 9, page 9, page 31., IC Engineering Department, Fujitsu Ltd., Jaapan