Abstract

The invention is related to non-linear, paraffin-soluble olefin/carbon monoxide and olefin/acetylene/carbon monoxide copolymers. The invention is also related to a method for preparing olefin/carbon monoxide copolymers by heating a feed of at least one olefin, carbon monoxide, carbon dioxide, hydrogen, and methane in the presence of a free radical polymerization initiator. More particularly, the feed comprises at least one olefin, the total olefin amount ranging from about 5 to about 40 mole %, carbon monoxide in an amount ranging from about 1 to about 40 mole %, hydrogen in an amount ranging from about 4 to about 55 mole %, carbon dioxide in an amount ranging from about 3 to about 10 mole %, and methane in an amount ranging from about 4 to about 85 mole %. The feed may also include acetylene in an amount ranging up to about mole %.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A composition comprising a non-linear, paraffin-soluble copolymer.

  2. Claim 2Depends on #1

    The composition of claim 1 wherein the copolymer's number average molecular weight ranges from about 200 to about 1,000.

  3. Claim 3Depends on #2

    The composition of claim 2 wherein CO incorporation in the copolymer ranges from about 2 to about 50 mole %.