Patents
US 6,156,629 A#1176641 Most CitedExpiredUnited States (USPTO)Utility

Method for patterning a polysilicon gate in deep submicron technology

44Forward Citations (#1176641 Global)
1.7/yrCitation Velocity (#2820673 Global)
6.98Citation PageRank (#1922103 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of etching polysilicon using an oxide hard mask using a three step etch process. Steps one and two are performed insitu in a high density plasma (e.g., TCP--transformer coupled plasma) oxide etcher. Step 3, the polysilicon etch is performed in a different etcher (e.g., poly RIE etcher). A multi-layered semiconductor structure 35 (FIG. 1) is formed comprising: a substrate 10, a gate oxide layer 14, a polysilicon layer 18, a hard mask layer 22, and a bottom anti-reflective coating (BARC) layer 26 and a resist layer 30. a) in STEP 1, etching the bottom anti-reflective coating (BARC) layer and the hard mask layer by flowing fluorocarbon gas species gas and argon gas, and applying a first TCP Power and a first Bias power; b) in STEP 2, stripping the bottom anti-reflective coating (BARC) layer by flowing a oxygen; and applying a second TCP Power and second Bias power; c) Placing the substrate into a polysilicon high density plasma etcher and performing the following step: in STEP 3--etching the polysilicon layer by flowing chlorine species, oxygen species; Helium species and bromine gas species and applying a third TCP Power and a third Bias power.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 44.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of fabrication of a polysilicon gate; comprising the steps of: forming sequentially a gate oxide layer, a polysilicon layer, a hard mask layer composed of silicon oxide, and a bottom anti-reflective coating (BARC) layer over a substrate; forming a resist layer over said bottom anti-reflective coating (BARC) layer; said resist layer defining said polysilicon gate; placing said substrate into an oxide high density plasma etcher and performing the following steps: a) in STEP 1, etching said bottom anti-reflective coating (BARC) layer and said hard mask layer by flowing fluorocarbon

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗