US 6,156,080 A#7481500 Most CitedExpiredUnited States (USPTO)Utility

Method of fabricating an electrode used for a prismatic cell

13Forward Citations (#7481500 Global)
0.5/yrCitation Velocity (#15218505 Global)
2.78Citation PageRank (#8547605 Global)
14Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

There is provided a method of fabricating an electrode used for a prismatic cell, including the steps of (a) winding an electrode sheet around a core, the electrode sheet comprising a positive electrode in the form of a sheet, a negative electrode in the form of a sheet, and an insulating sheet sandwiched between the positive and negative electrodes, (b) pulling out the core to thereby form a wound electrode sheet deposition, (c) heating the wound electrode sheet deposition at a temperature equal to or lower than a melting temperature of the insulating sheet for 30 minutes or smaller, and (d) compressing the wound electrode sheet deposition with a uniaxial pressure to thereby flatten the wound electrode sheet deposition. In accordance with the above-mentioned method, it is possible to increase a cell capacity per a unit volume in a prismatic cell, because the electrode sheet can be wound further half turn or a plurality of times. In addition, it is also possible to increase an efficiency in a charging and discharging cycle, because a gap between the electrodes and the insulating sheet is made smaller, and a space in a center of the wound electrode sheet deposition is also made smal

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 13.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating an electrode used for a prismatic cell, comprising the steps of: (a) winding an electrode sheet around a core, said electrode sheet comprising a positive electrode in the form of a sheet, a negative electrode in the form of a sheet, and an insulating sheet sandwiched between said positive and negative electrodes; (b) pulling out said core to thereby form a wound electrode sheet deposition; and (c) simultaneously compressing and heating said wound electrode sheet deposition, to thereby flatten said wound electrode sheet deposition.

  2. Claim 2Depends on #1

    The method as set forth in claim 1, wherein said wound electrode sheet deposition is kept compressed for a period of time ranging from 5 seconds to 180 seconds in said step (c).

  3. Claim 3Depends on #1

    The method as set forth in claim 1, wherein said wound electrode sheet d