Abstract

PCT No. PCT/JP98/05242 Sec. 371 Date Sep. 16, 1999 Sec. 102(e) Date Sep. 16, 1999 PCT Filed Nov. 20, 1998 PCT Pub. No. WO99/37466 PCT Pub. Date Jul. 29, 1999A biaxially oriented polyester film for a membrane switch, which is made from a polyester containing at least 80 mol % of ethylene-2,6-naphthalene dicarboxylate recurring units and which has an endothermic peak with an endothermic energy of at least 0.4 mJ/mg at a temperature of 110 to 160 DEG C. This film is produced by subjecting a biaxially oriented polyester film produced from the above polyester in accordance with a method known per se to the following steps in the order named: (1) the step of heating the film under no strain at a temperature of 150 to 180 DEG C. for 1 to 5 hours; and (2) the step of heating the film in an unrolled or rolled state at a temperature of 80 to 122 DEG C. for 5 to 200 hours.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 30.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A biaxially oriented polyester film for a membrane switch, (A) which comprises a polyester containing at least 80 mol % of ethylene-2,6-naphthalene dicarboxylate recurring units, and (B) which has an endothermic peak with an endothermic energy of at least 0.4 mJ/mg at a temperature of 110 to 160° C.

  2. Claim 2Depends on #1

    The biaxially oriented polyester film of claim 1, wherein the polyester (A) contains at least 85 mol % of ethylene-2,6-naphthalene dicarboxylate recurring units.

  3. Claim 3Depends on #1

    The biaxially oriented polyester film of claim 1, wherein the polyester (A) has an intrinsic viscosity of 0.40 to 0.90 dl/g.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • International Search Report.
  • Taiwan Office Action dated Nov. 24, 1999.