Integrated CVD/PVD Al planarization using ultra-thin nucleation layers
Abstract
The present invention provides a method and apparatus for forming an interconnect with application in small feature sizes (such as quarter micron widths) having high aspect ratios. Generally, the present invention provides a method and apparatus for depositing a wetting layer for subsequent physical vapor deposition to fill the interconnect. In one aspect of the invention, the wetting layer is a metal layer deposited using either CVD techniques or electroplating, such as CVD aluminum (Al). The wetting layer is nucleated using an ultra-thin layer, denoted as +531 layer, as a nucleation layer. The +531 layer is preferably comprised of a material such as Ti, TiN, Al, Ti/TiN, Ta, TaN, Cu, a flush of TDMAT or the like. The +531 layer may be deposited using PVD or CVD techniques, preferably PVD techniques to improve film quality and orientation within the feature. Contrary to conventional wisdom, the +531 layer is not continuous to nucleate the growth of the CVD wetting layer thereon. A PVD deposited metal is then deposited on the wetting layer at low temperature to fill the interconnect.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 19.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for processing a substrate, comprising: (a) introducing the substrate into a first process zone; (b) depositing a dis-continuous nucleation layer having scattered nucleation sites within vias on the substrate; (c) introducing the substrate into a second process zone; (d) depositing a wetting layer on the dis-continuous nucleation layer; (e) introducing the substrate into a third process zone; and (f) depositing a conducting laster on the wretting layer.
- Claim 2Depends on #1
The method of claim 1, wherein the depositing a dis-continuous nucleation layer comprises depositing a dis-continuous layer selected from the group consisting of Ti, TiN, Ta, TaN, Al, Cu, TDMAT, and combinations thereof.
- Claim 3Depends on #2
The method of claim 2, wherein the dis-continuous nucleation layer is deposited by physical vapor depositing a dis-co
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 19 total)
References Cited — Backward Prior Art (29)
Non-Patent Literature (5)
- European Search Report dated May 27, 1999.
- K. Mikagi, H. Ishikawa, T. Usami, M. Suzuki, K. Inoue, N. Oda, S. Chikaki, I. Sakai and T. Kikkawa, "Barrier Metal Free Copper Damascene Interconnection Technology Using Atmospheric Copper Reflow and Nitrogen Doping in SiOF Film," 1996 IEEE, pp. 365-368.
- K. Mikagi, H. Ishikawa, T. Usami, M. Suzuki, K. Inoue, N. Oda, S. Chikaki, I. Sakai and T. Kikkawa, Barrier Metal Free Copper Damascene Interconnection Technology Using Atmospheric Copper Reflow and Nitrogen Doping in SiOF Film, 1996 IEEE, pp. 365 368.
- Li, et al., "Copper Deposition and Thermal Stability Issues in Copper-Based Metalization for ULSI Technology," Materials Science Reports, 1992, Vol. 9, pp. 1-51.
- Li, et al., Copper Deposition and Thermal Stability Issues in Copper Based Metalization for ULSI Technology, Materials Science Reports, 1992, Vol. 9, pp. 1 51.