Abstract
A method and apparatus for deburring or radiusing articles made of TZM alloys by electrochemical machining uses a pulsating current and a binary salt electrolyte solution simultaneously applied across a gap between a tool electrode and a TZM workpiece. The pulse duration is typically in the range between about 0.5 milliseconds to about 100 milliseconds and the pulse interval is between 5 milliseconds and 150 milliseconds. The pulse voltage amplitude is typically in the range between about 8 volts to about 30 volts. The binary salt electrolyte solution is an aqueous salt solution with a total concentration typically in the range between about 14% to about 20% by weight of sodium chloride and sodium nitrate. The ratio of sodium chloride to sodium nitrate is typically in the range of between about 1:1 to about 1.5:1. The standoff distance, or gap, between the tool electrode and the TZM workpiece is typically in the range between 0.015 mm to about 3.0 mm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 14.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for electrochemical deburring or radiusing of a TZM workpiece with a tool electrode, poled to cause said tool electrode to act as a cathode and said TZM workpiece to act as an anode, said method comprising: directing a binary salt electrolyte solution comprising aqueous sodium chloride and sodium nitrate through a gap between said tool electrode and said TZM workpiece; and applying a pulsating current across said gap.
- Claim 2Depends on #1
The method as claimed in claim 1 wherein said binary salt electrolyte solution has a compound concentration between about 14% to about 20% by weight of sodium chloride and sodium nitrate in water.
- Claim 3Depends on #2
The method as claimed in claim 2 wherein said binary salt electrolyte solution has a ratio of sodium chloride to sodium nitrate in a range between 1:1 to about 1.5:1.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (5)
- B. Wei et al., "Pulse ECM of Titanium Alloy Ti-6A1-4V", Transactions of NAMRI/SME, XXII, North American Manufacturing Research Institutes of the Society of Manufacutirng Engineers, 1994, p. 141, (No Month).
- B. Wei et al., Pulse ECM of Titanium Alloy Ti 6A1 4V , Transactions of NAMRI/SME, XXII, North American Manufacturing Research Institutes of the Society of Manufacutirng Engineers, 1994, p. 141, (No Month).
- C. Yu et al., "The Relation Between Copying Accuracy and Electrolytes of ECM for Titanium Alloy", Annals of the CIRP, vol. 30, Jan. 1981, p. 123.
- C. Yu et al., The Relation Between Copying Accuracy and Electrolytes of ECM for Titanium Alloy , Annals of the CIRP, vol. 30, Jan. 1981, p. 123.
- C. Zhou et al., "Electrochemical Machining of Hard Passive Alloys With Pulse Reverse Current", NAMRI/SME, XXV, 1997, p. 147, (No Month).