Methods to improve copper-fluorinated silica glass interconnects
Abstract
A method of forming an interconnect, comprising the following steps. A semiconductor structure is provided that has an exposed first metal contact and a dielectric layer formed thereover. An FSG layer having a predetermined thickness is then formed over the dielectric layer. A trench, having a predetermined width, is formed within the FSG layer and the dielectric layer exposing the first metal contact. A barrier layer, having a predetermined thickness, may be formed over the FSG layer and lining the trench side walls and bottom. A metal, preferably copper, is then deposited on the barrier layer to form a copper layer, having a predetermined thickness, over said barrier layer covered FSG layer, filling the lined trench and blanket filling the barrier layer covered FSG layer. The copper layer, and the barrier layer on said upper surface of said FSG layer, are planarized, exposing the upper surface of the FSG layer and forming a planarized copper filled trench. The FSG layer and planarized copper filled trench are then processed by either: (1) annealing from about 400 to 450° C. for about one hour, then either NH 3 or H 2 plasma treating; or (2) Ar + sputtering to ion implant Ar + to
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 118.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming an interconnect, comprising the steps of: providing a semiconductor structure having an exposed first metal contact; forming a dielectric layer having a predetermined thickness over said semiconductor structure; forming a fluorinated silica glass layer having a predetermined thickness over said dielectric layer; forming a trench within said fluorinated silica glass layer and said dielectric layer exposing said first metal contact, said trench having a predetermined width; forming a second metal layer filling said trench and blanket filling said fluorinated silica gl
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 118 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (5)
- Peters, "Pursuing the Perfect Low-k Dielectric", Semiconductor International, Sep. 1998, pp. 64-74.
- Peters, Pursuing the Perfect Low k Dielectric , Semiconductor International, Sep. 1998, pp. 64 74.
- Swope et al., "Improvement of Adhesion Properties of Fluorinated Silica Glass Films by Nitrous Oxide Plasma Treatment", Journal Electrochem. Soc., vol. 144, No. 7, Jul. 1997, pp. 2559-2564.
- Swope et al., Improvement of Adhesion Properties of Fluorinated Silica Glass Films by Nitrous Oxide Plasma Treatment , Journal Electrochem. Soc., vol. 144, No. 7, Jul. 1997, pp. 2559 2564.
- Yang et al., "The Stability of Si-O-F low-k dielectrics: Attack by water molecules as function of near-neighbor Si-F bonding arrangements", J. Vacuum Sci. Technol., A 16(3), May/Jun. 1998, pp. 1525-1527.