Patents
US 6,136,672 A#3299969 Most CitedExpiredUnited States (USPTO)Utility

Process for device fabrication using a high-energy boron implant

24Forward Citations (#3299969 Global)
0.9/yrCitation Velocity (#7769567 Global)
2.44Citation PageRank (#10572490 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for semiconductor device fabrication in which a Czochralski silicon substrate is implanted with boron is disclosed. The boron is implanted using an energy of about 500 keV to about 3 MeV and a dose of about 3x1013/cm2 to about 3x1014/cm2. In order to reduce the threading dislocation density in the substrate to less than about 103/cm2 at a depth in the substrate of at least about 0.5 mu m, after the implant, the substrate is annealed in a two-step process. First the substrate is annealed at a temperature in the range of about 725 DEG C. to about 775 DEG C. followed by an anneal at a temperature of at least about 900 DEG C. The duration of the first step is selected to provide a dislocation density of less than about 103/cm2 at the desired depth in the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 24.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for device fabrication comprising: implanting a boron dopant into a Czochralski (Cz) silicon substrate wherein the implant energy is in the range of about 500 keV to about 3 MeV and the implant dose is about 1×10 13 atoms/cm 2 to about 5×10 14 atoms/cm 2 ; annealing the implanted substrate at a first temperature followed by a second temperature to distribute the dopant in the substrate wherein the first temperature is about 725° C. to about 800° C. and the second temperature is at least about 900° C. and wherein the duration of the anneal at the first temperature is less than a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Anonmalous Leakage Current Reduction by Ramping Rate Control in MEV Impantation", by Hamada, K. et al. Mat. Res. Symp. Proc., vol. 396, pp. 739-743 (1996).
  • "Bipolar Transistor with a Buried Layer Formed yb High-Energy Ion Implantation for Subhalf-Micron Bipolar-Complementary Metal Oxide Semiconductor LSIs", by Kuroi, T. et al., Japan J. Appl. Phys., 33, pp. 541-545 (1994).
  • "Formation of Extended Defects in Silicon by High Energy Implantation of B and P", by Cheng, J. Y. et al., J. Appl. Phys., 80 (4), pp. 2105-2112 (Aug. 15, 1996).
  • "High Energy Ion Implantation for ULSI: Well Engineering and Gettering", by Tsukamoto, K. et al., Solid state Technology, pp. 49-51 (Jun. 1992).
  • "High-Energy Ion Implantation for ULSI", by Tsukamoto, K. et al., Nuclear Instruments and Methods in Physics-Research, B59/60, pp. 584-591 (1991).