Filling of high aspect ratio trench isolation
Abstract
A method of forming a trench isolation on a semiconductor substrate comprising the steps of forming a trench in the substrate, partially filling the trench with a first layer of polysilicon, oxidizing the first layer of polysilicon, partially filling the trench with at least a second layer of polysilicon, and oxidizing the second layer of polysilicon. By utilizing the method of the present invention, formation of voids and defects in a trench isolation having a high aspect ratio can be prevented.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 74.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming a trench isolation on a semiconductor substrate, comprising the steps of: forming a trench in said substrate, the trench having side walls and a bottom; partially filling said trench with a first layer of silicon, so that the bottom of the trench is covered by said first layer of silicon; oxidizing said first layer of silicon, so that the bottom of the trench is covered by an oxide of silicon; partially filling said trench with at least a second layer of silicon; and oxidizing said second layer of silicon, wherein said trench is partially filled with said second l
- Claim 2Depends on #1
The method, as recited in claim 1, further comprising the step of forming a layer of nitride in said trench prior to filling said trench with said layers of silicon.