Patents
US 6,133,413 A#3039309 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing devulcanized rubber using high temperature and shearing pressure

25Forward Citations (#3039309 Global)
1.0/yrCitation Velocity (#7504054 Global)
3.79Citation PageRank (#5199525 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Devulcanized rubber in which sulfuric crosslinking bonds are cut and which contains carbon black particles having very small diameters. Vulcanized rubber of discarded products is devulcanized by heating it at a temperature of 180 DEG C. -350 DEG C. and applying a shearing pressure of 10-150 kg/cm2 thereto. Reclaimed rubber products are manufactured by vulcanizing and molding, into desired shapes, a material made of only devulcanized rubber in which sulfuric crosslinking bonds are cut and which contains carbon black particles having very small diameters or a material made of the devulcanized rubber mixed with virgin unvulcanized rubber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 25.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing devulcanized rubber comprising rubber with sulfur crosslinks thereof severed and carbon black particles of 100 nm or less in diameter comprising the steps of: (a) pulverizing vulcanized rubber selected from the group consisting of EPDM (ethylene-propylene-diene terpolymer) rubber, natural rubber, styrene-butadiene rubber and butyl rubber containing carbon black; (b) heating the pulverized vulcanized rubber containing carbon black in the temperature range of 280° C. to 330° C. when the rubber is EPDM rubber, 200° C. to 270° C. when the rubber is natural rubber, 200°