Patents
US 6,133,330 A#1419687 Most CitedExpiredUnited States (USPTO)Utility

Aromatic polyimide foam

40Forward Citations (#1419687 Global)
1.5/yrCitation Velocity (#3339164 Global)
3.71Citation PageRank (#5377405 Global)
10Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A mechanically undensified aromatic polyimide foam is made from an aromatic polyimide precursor solid residuum and has the following combination of properties: a density according to ASTM D-3574A of about 0.5 pounds/ft3 to about 20 pounds/ft3; a compression strength according to ASTM D-3574C of about 1.5 psi to about 1500 psi; and a limiting oxygen index according to ASTM D-2863 of about 35% oxygen to about 75% oxygen at atmospheric pressure. The aromatic polyimide foam has no appreciable solid inorganic contaminants which are residues of inorganic blowing agents. The aromatic polyimide which constitutes the aromatic polyimide foam has a glass transition temperature (Tg) by differential scanning calorimetry of about 235 DEG C. to about 400 DEG C.; and a thermal stability of 0 to about 1% weight loss at 204 DEG C. as determined by thermogravimetric analysis (TGA). The aromatic polyimide foam has utility as foam insulation and as structural foam, for example, for aeronautical, aerospace and maritime applications.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 40.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A mechanically undensified foam comprising an aromatic polyimide and having the following combination of properties: a density according to ASTM D-3574A of from about 0.5 pounds/ft 3 to about 20 pounds/ft 3 ; a compression strength according to ASTM D-3574C of from about 1.5 psi to about 1500 psi; and a limiting oxygen index according to ASTM D-2863 of from about 35% oxygen to about 75% oxygen at atmospheric pressure; the foam having no appreciable solid inorganic contaminants which are residues of inorganic blowing agents.

  2. Claim 2Depends on #1

    The foam of claim 1, wherein the aromatic polyimide has a glass transition temperature (Tg) by differential scanning calorimetry of from about 235° C. to about 400° C.; and a thermal stability of from 0 to about 1% weight loss at 204° C. as determined by thermogravimetric analysis (TGA). 3

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • WPI/Derwent 1977 243843 Abstract.
  • WPI/Derwent 1977-243843 Abstract.