Low temperature process for fabricating layered superlattice materials and making electronic devices including same
Abstract
A liquid precursor containing thallium is applied to a first electrode, RTP baked at a temperature lower than 725° C., and annealed at the same temperature for a time period from one to five hours to yield a ferroelectric layered superlattice material. A second electrode is formed to form a capacitor, and a second anneal is performed at a temperature lower than 725° C. If the material is strontium bismuth thallium tantalate, the precursor contains (m-1) mole-equivalents of strontium for each of (2.2-x) mole-equivalents of bismuth, x mole-equivalents of thallium, and m mole-equivalents of tantalum, where m=2 and 0.0<x≦2.2.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 10.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of fabricating a ferroelectric device in an integrated circuit comprising the steps of: providing a substrate, and a precursor containing metal moieties in effective amounts for spontaneously forming a ferroelectric layered superlattice material upon drying and heating of said precursor, wherein said precursor contains metal moieties in amounts corresponding to the general formula A m-1 (S1 y-x S2 x )B m O 3m+3 , wherein S1 represents bismuth, S2 represents thallium, 2≦y≦2.4 and 0<x≦y; applying said precursor to said substrate; drying said precursor to form a dried material
- Claim 2Depends on #1
A method as in claim 1 wherein A represents strontium an
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗