Titanium-based intermetallic alloys
Abstract
A titanium-based intermetallic alloy having a high yield stress, a high creep resistance and sufficient ductility at ambient temperature has the following chemical composition as measured in atomic percentages: Al, from 16 to 26; Nb, from 18 to 28; Mo, from 0 to 2; Si, from 0 to 0.8; Ta, from 0 to 2; Zr, from 0 to 2; and Ti as the balance to 100; with the condition that Mo+Si+Zr+Ta>0.4%. Production, working and heat-treatment ranges adapted to the intended use of the material are also defined.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 30.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A titanium-based intermetallic alloy having a composition, comprising: Al, from 16 to 26 atomic %; Nb, from 18 to 28 atomic %; Mo, from 0 to 2 atomic %; Si, from 0 to 0.8 atomic %; Ta, from 0 to 2 atomic %; Zr, from 0 to 2 atomic %; Ti, balance to 100 atomic %; wherein Mo+Si+Zr+Ta>0.4 atomic %; and wherein said alloy has an O phase structure.
- Claim 2Depends on #1
An intermetallic alloy as claimed in claim 1, produced by a process, comprising: a) melting of said composition to obtain an ingot of homogeneous composition having a grain structure; b) high-speed deforming resulting in a reduction in the grain size; c) isothermal forging at a temperature between a β transus temperature T.sub.β minus 125° C. and the β transus temperature T.sub.β minus 25° C., with a strain rate of between 5×10 -4 s -1 and 5×10 -2 s -1 ; and, d) heat