Method of making a fiber having low loss at 1385 nm by cladding a VAD preform with a D/d<7.5
Abstract
A singlemode optical fiber 700 having very low loss at 1385 nm, and a practical method for making same are disclosed. A core rod 20 is fabricated using vapor axial deposition to have a deposited cladding/core ratio (D/d) that is less than 7.5. The core rod is dehydrated in a chlorine- or fluorine-containing atmosphere at about 1200 DEG C. to reduce the amount of OH present to less than 0.8 parts per billion by weight, and then consolidated in a helium atmosphere at about 1500 DEG C. to convert the porous soot body into a glass. The consolidated core rod is elongated using an oxygen-hydrogen torch that creates a layer of OH ions on the surface of the rod that are largely removed by plasma etching. Finally, the core rod is installed in a glass tube 40 having a suitably low OH content. Thereafter, the tube is collapsed onto the rod to create a preform 60. Conventional methods are employed for drawing an optical fiber from the preform and applying one or more protective coatings 75, 76. The disclosed method is suitable for commercial production of low-OH fiber. Significantly, the fiber's loss at 1385 nm is reduced to a level that is less than its loss at 1310 nm, thereby rendering
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 109.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for making a singlemode optical fiber having low loss at 1385 nanometers (nm) including the following steps: forming a glass rod by soot deposition, said rod comprising a cylindrical core having a diameter (d) surrounded by a layer of deposited cladding material having a diameter (D), wherein D/d<7.5; dehydrating the glass rod in a chlorine- or fluorine-containing atmosphere at a temperature, which is less than 1300° C. in order to reduce the concentration of hydroxyl ions to a level that is less than about 0.8 parts per billion by weight; consolidating the glass rod at a tempe
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 109 total)
References Cited — Backward Prior Art (15)
Non-Patent Literature (5)
- F. Hanawa, et al., Fabrication of Completely OH Free V.A.D. Fibre, Electronics Letters, Aug. 28, 1980, vol. 16, No. 18, 699 700.
- F. Hanawa, et al., Fabrication of Completely OH-Free V.A.D. Fibre, Electronics Letters, Aug. 28, 1980, vol. 16, No. 18, 699-700.
- Hanawa, et al., "Tunable Magnetostatic Surface Wave Demultiplexing Fiber/Switch," Electronics Letters, Aug. 1980, vol. 16, No. 18, 699-700.
- Hanawa, et al., Tunable Magnetostatic Surface Wave Demultiplexing Fiber/Switch, Electronics Letters , Aug. 1980, vol. 16, No. 18, 699 700.
- K. Kosaka, et al., "Fabrication of ultralow-loss and low-OH VAD single-mode fibers," in Proc, 10th ECOC, Sep., 1984, pp. 292-293.