Patents
US 6,124,409 A#7858189 Most CitedExpiredUnited States (USPTO)Utility

Processes for preparing copolymers

13Forward Citations (#7858189 Global)
0.5/yrCitation Velocity (#15522878 Global)
1.65Citation PageRank (#19801662 Global)
14Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed is a process for preparing copolymers which comprises, in the order stated: (1) adding monomers containing unsaturated carbon-to-carbon bonds, a first polymerization initiator, a second polymerization initiator, and a solvent to a reaction vessel; (2) purging the resulting solution with an inert gas; (3) sealing the reaction vessel and pressurizing it by addition of an inert gas to a pressure of from about 20 to about 600 kilopascals over ambient atmospheric pressure; (4) maintaining the temperature within the pressurized reaction vessel at a temperature of from about 50 to about 100° C. for a period of from about 60 to about 300 minutes; (5) thereafter maintaining the temperature within the pressurized reaction vessel at a temperature of from about 80 to about 115° C. for a period of from about 30 to about 300 minutes, wherein the temperature in step (5) is higher than the temperature in step (4); and (6) subsequently maintaining the temperature within the pressurized reaction vessel at a temperature of from about 115 to about 160° C. for a period of from about 30 to about 180 minutes, wherein the temperature in step (6) is higher than the temperature in step (5). Polyme

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing copolymers which comprises, in the order stated: (1) adding monomers containing unsaturated carbon-to-carbon bonds, two polymerization initiators, namely a first polymerization initiator with a 10 hour half-life temperature of from about 50° C. to about 95° C. and a second polymerization initiator with a 10 hour half-life temperature of from about 85° C. to about 130° C., and a solvent to a reaction vessel; (2) subsequent to step 1, purging the resulting solution with an inert gas; (3) subsequent to step 2, sealing the reaction vessel and pressurizing it by addition of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Reactivity, Mechanism and Structure in Polymer Chemistry, ed. A. D. Jenkins and A. Ledwith, John Wiley, New York, 1974, pp. 158 174.
  • Reactivity, Mechanism and Structure in Polymer Chemistry, ed. A. D. Jenkins and A. Ledwith, John Wiley, New York, 1974, pp. 158-174.