Thermoplastic coating compositions and process using same

15Forward Citations (#6363438 Global)
0.6/yrCitation Velocity (#13644053 Global)
2.51Citation PageRank (#10107401 Global)
19Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This invention provides for a coating composition comprising: (A) at least one polymeric material selected from (i) at least one homopolymer of ethylene having a melt index of at least about 220 grams per ten minutes as determined by ASTM D1238, condition 190/2.16, or (ii) at least one copolymer of ethylene and a second ethylenically unsaturated monomer having a melt index of at least about 20 grams per ten minutes as determined by ASTM D1238, condition 190/2.16, or (iii) at least one thermoplastic acrylic homopolymer or copolymer having a glass transition temperature (Tg) of greater than 0° C. but less than 110° C., or (iv) a mixture of (i), (ii) and/or (iii); and (B) at least one thermoplastic polymeric material different than (A) having a melting point in the range of about 80° C. to about 130° C. and being miscible with (A) and wherein the viscosity of the polymer composition (A) and (B) is in the range of about 5,000 cps to about 100,000 cps at a temperature range of about 200° F. to about 300° F. The invention further provides for a process for applying the foregoing coating composition to a substrate such as glass, ceramic, metal, fiberboard, textile or plastic substrate (e.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 15.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A printing coating composition for forming a decorative coating on a substrate comprising: (A) (i) at least one homopolymer of ethylene having a melt index of at least about 220 grams per ten minutes as determined by ASTM D1238, condition 190/2.16, or (ii) at least one copolymer of ethylene and a second ethylenically unsaturated monomer having a melt index of at least about 20 grams per ten minutes as determined by ASTM D1238, condition 190/2.16, or (iii) at least one thermoplastic acrylic homopolymer or copolymer having a glass transition temperature (Tg) of greater than 0° C. but less than 1

Technical Overview & Description