Patents
US 6,121,402 A#278767 Most CitedExpiredUnited States (USPTO)Utility

Polyethylene, thermoplastic resin composition containing same, and process for preparing polyethylene

93Forward Citations (#278767 Global)
3.6/yrCitation Velocity (#603940 Global)
6.36Citation PageRank (#2240698 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Polyethylenes are disclosed herein which are derived from an ethylene monomer and in which any quaternary carbon atom is not present in a polymeric main chain; and the activation energy (Ea) of melt flow is in the range of 8 to 20 kcal/mol; as well as (1) a Huggins coefficient (k) and an intrinsic viscosity [ eta ] meet the relation of the equationk>/=0.2+0.0743x[ eta ];(2) a molar ratio [CH3/CH2] of a methyl group to a methylene group is in a region of 0.005 to 0.1 and meets the equationTm>/=131-1340[CH3/CH2];(3) an Mw and a die swell ratio (DR) meet the equationDR>0.5+0.125xlog Mw; or(4) in the measurement of a loss elastic modulus, a beta -relaxation peak is present in the range of 0 to -100 DEG C. These polyethylenes are different from a usual HDPE, L-LDPE and LDPE, and they are excellent in working properties and permit the control of physical properties such as density, a melting point and crystallinity mainly in the state of a homopolymer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 93.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A polyethylene derived from an ethylene monomer in which (1) a quaternary carbon atom is not present in a polymeric main chain; (2) the activation energy (Ea) of the melt flow is in the range of 8-20 kcal/mol.; (3) a Huggins coefficient (k) and an intrinsic viscosity (η) which are decided by the relation between a polymer concentration and a reduced viscosity measured at a temperature of 135 ° C. in a decalin solvent meet the relationship of the equation: k≧0.2+0.0743×(η); and (4) in the measurement of a loss elastic modulus, a β-relaxation peak is present in the range of 0 to -100° C.

  2. Claim 2Depends on #1

    The polyethylene according to claim 1, wherein a density (D) is in the range of 0.86 to 0.95 g/cm 3 , and a crystallization enthalpy (ΔH) and a melting point (Tm) measured by a differential scanning calorimeter (DSC) meet the equation 0≦ΔH≦250

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗