Patents
US 6,103,188 A#12203337 Most CitedExpiredUnited States (USPTO)Utility

High-conductivity copper microalloys obtained by conventional continuous or semi-continuous casting

9Forward Citations (#12203337 Global)
0.3/yrCitation Velocity (#22439827 Global)
1.55Citation PageRank (#21689283 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

We provide a new copper microalloy with high-conductivity, excellent heat resistance and high strain strength, which can be obtained by conventional continuous or semi-continuous casting, which essentially consists of at least one element selected from the following list: ______________________________________ 5-800 mg/Kg Pb (lead) 10-100 mg/Kg Sb (antimony) 5-1000 mg/Kg Ag (silver) 5-700 mg/Kg Sn (tin) 1-25 mg/Kg Cd (cadmium) 1-30 mg/Kg Bi (bismuth) 20-500 mg/Kg Zn (zinc) 10-400 mg/Kg Fe (iron) 15-500 mg/Kg Ni (nickel) 1-15 mg/Kg S (sulfur) ______________________________________ in all cases, with 20-500 mg/Kg O (oxygen). The alloy is suitable for all the applications that require an electrical conductivity similar to that of pure copper, but with a better heat resistance, better mechanical properties and lower standard deviation values in strain strength. Specifically, it can be used for electric wires with high mechanical requirements and/or high annealing temperatures, for high-risk applications and for electrical wires and components in the electronic and micro-electronic industry.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A high-conductivity copper alloy, consisting essentially of (4N) Cu and at least one element selected from the group consisting of: 5-800 mg/Kg lead, 10-100 mg/Kg antimony, 5-1000 mg/Kg silver, 5-700 mg/Kg tin, 20-500 mg/Kg zinc, 1-25 mg/Kg cadmium, 1-30 mg/Kg bismuth, 10-400 mg/Kg iron, 1-15 mg/Kg sulfur, and 15-500 mg/Kg nickel, in which oxygen must be present at a concentration of between 20 and 500 mg/Kg.

  2. Claim 2Depends on #1

    A wire made of the copper alloy described in claim 1.

  3. Claim 3Depends on #1

    A high mechanical requirements electric rod or wire with high electrical conductivity (at least 99% IACS) made of the copper alloy described in claim 1.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗