US 6,096,478 A#10776501 Most CitedExpiredUnited States (USPTO)Utility

Resist material for forming a chemically amplified negative type resist pattern and method of manufacturing a semiconductor device employing the resist pattern

10Forward Citations (#10776501 Global)
0.4/yrCitation Velocity (#21100211 Global)
1.68Citation PageRank (#19193791 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An object of the present invention is to inhibit a size difference possibly caused due to different pattern densities, and at the same time to form a desired resist having fewer irregularities on the side walls thereof, all with respect to a chemically amplified negative type resist. In order to achieve the object, a resist material of the present invention comprises a resin for forming the resist material, a first photo-acid generating agent having a molecular weight of 100-1000 and capable of producing an acid having a diffusion length of 10-30 nm, a second photo-acid generating agent having a molecular weight of 100-1000 and capable of producing an acid having a diffusion length of 30-60 nm. In particular, a mixing ratio for mixing the second photo-acid generating agent into the first photo-acid generating agent is 5-95 mol %, a mixing ratio for mixing a total amount of the first and second photo-acid generating agents into the resin is 1-15 wt %.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A resist material, comprising: a resin for forming the resist material; a first photo-acid generating agent having a molecular weight between 100 and 1000 and producing a photo-acid having a diffusion length between 10 and 30 nm by exposure; and a second photo-acid generating agent having a molecular weight between 100 to 1000 and producing an photo-acid having a diffusion length between 30 and 60 nm by exposure, the second photo-acid generating agent being mixed into the first photo-acid generating agent at a ratio between 5 and 95 mol %, the first and the second photo-acid agents bei

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Hashimoto et al. Microelectronic Eng. 41/42, 1998, 363 366.
  • Hashimoto et al. Microelectronic Eng. 41/42, 1998, 363-366.
  • JP 10223503A, Aug. 1998, Derwent Abstract.
  • JP 10223503A, Aug.-1998, Derwent Abstract.