Patents
US 6,093,333 A#26969916 Most CitedExpiredUnited States (USPTO)Utility

Method for etching thin nickel iron film to make a magnetic recording head

4Forward Citations (#26969916 Global)
0.1/yrCitation Velocity (#38697626 Global)
1.13Citation PageRank (#35212981 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In the formation of a magnetic recording head or other electronic device on a substrate, at least one thin nickel iron-film is deposited on the substrate and an element is formed by etching the film. The film is first activated by disposing the film in a hydrochloric acid activating solution containing a ferrous salt. After activation, the film is removed from the activating solution and the hydrochloric acid rinsed away from the substrate. Then, the film is etched by disposing it in a sulfuric acid bath containing a ferric salt. After etching, the film is rinsed with sulfuric acid. The process substantially avoids residual corrosion of the resulting head that otherwise would be caused by chloride lingering in the etched portions of the head.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a magnetic recording head from a substrate that supports a nickel-iron thin film layer, comprising: disposing the thin film layer in a hydrochloric acid activation bath containing a reducing agent; removing the thin film layer from the activation bath; rinsing the thin film layer to remove hydrochloric acid therefrom; and disposing the thin film layer in an acidic, substantially chloride-free ferric etching bath to etch the thin film layer.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the thin film layer, except for the predetermined portions thereof, is covered with a protective layer.

  3. Claim 3Depends on #2

    The method of claim 2, wherein the activation bath includes a surfactant.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Active-State Dissolution of 50N and 79NM Iron-Nickel Alloys in Phosphoric Acid Solutions", Trepak, N.M., Il'ina, L..K., and L'vov, A..L., N.G. Chernyshevskii Saratov State University, translated from Elektrokhimiya, vol. 20, No. 4, pp. 526-529, Apr. 1984.
  • "Electrochemical Aspects of the Beveling of Sputtered Permalloy Foims", Kelly, J.J. and Koel, G.J., Electrochemical Science & Technology, vol. 125, No. 6, Jun. 1978, pp. 860-865.
  • "On the Preferred Dissolution of Iron from Thin Films of Permalloy", Kohler, M., Wiegand, A. and Lerm, A., Journal of the Electrochemical Society, Accelerated Brief Communications, pp. 2293-2294, Sep. 1985.
  • Active State Dissolution of 50N and 79NM Iron Nickel Alloys in Phosphoric Acid Solutions , Trepak, N.M., Il ina, L..K., and L vov, A..L., N.G. Chernyshevskii Saratov State University, translated from Elektrokhimiya, vol. 20, No. 4, pp. 526 529, Apr. 1984.
  • Description of Hungarian Patent 174,472, Nov. 5, 1995.