Patents
US 6,090,874 A#31615625 Most CitedExpiredUnited States (USPTO)Utility

High clarity carboxylated nitrile rubber

3Forward Citations (#31615625 Global)
0.1/yrCitation Velocity (#43129851 Global)
1.14Citation PageRank (#34662998 Global)
1Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a high clarity water-sensitive carboxylated nitrile rubber composition which is particularly useful in making photopolymer formulations for printing plates utilized in flexographic printing applications. The present invention more specifically discloses a high clarity water-sensitive carboxylated nitrile rubber composition which is comprised of (a) a carboxylated nitrile rubber which is comprised of repeat units which are derived from about 33 weight percent to about 77 weight percent 1,3-butadiene, from about 15 weight percent to about 45 weight percent acrylonitrile and from about 8 weight percent to about 22 weight percent methacrylic acid and (b) from about 1 to about 10 phr of at least one organic acid which contains at least three carboxyl groups. The carboxylated nitrile rubber of this invention will typically have a Mooney ML-4 viscosity of less than about 80 and a volume swell of greater than 40 percent. It will also have sufficient clarity to allow print having 6-point font to be read through a 0.125-inch thick sheet of said carboxylated nitrile rubber. In applications where improved scorch safety is required, the rubber composition will a

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a high clarity water-sensitive carboxylated nitrile rubber composition which comprises the steps of (1) free radical polymerizing from about 30 weight percent to about 73 weight percent 1,3-butadiene, from about 20 weight percent to about 50 weight percent acrylonitrile and from about 7 weight percent to about 20 weight percent methacrylic acid in an aqueous polymerization medium in the presence of at least one emulsifier to produce a carboxylated nitrile rubber latex; (2) adjusting the pH of the carboxylated nitrile rubber latex to above 4 by the addition of a base to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (1)