Patents
US 6,090,686 A#6942266 Most CitedExpiredUnited States (USPTO)Utility

Locos isolation process using a layered pad nitride and dry field oxidation stack and semiconductor device employing the same

14Forward Citations (#6942266 Global)
0.5/yrCitation Velocity (#14725286 Global)
2.49Citation PageRank (#10256988 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention provides methods of manufacturing a field oxide isolation structure over a semiconductor. One of the methods includes the steps of: (1) depositing a first stack-nitride sublayer over the semiconductor at a first deposition rate and (2) subsequently depositing a second stack-nitride sublayer over the first stack-sublayer at a second deposition rate that is either greater or less than the first deposition rate. The first and second deposition rates provide first and second stack-nitride sublayers that cooperate to form a relatively thin, uniform thickness of the field oxide isolation structure over the semiconductor and provide a stress-accommodating system within the semiconductor. The varying rates of deposition and accompanying changes in mixture ratio, produce a stack that is better able to absorb stress, has greater uniformity and is far less subject to the disadvantageous phenomenon of stack-lifting, particularly encountered in semiconductor having a PADOX layer deposited thereon.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 14.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing an isolation structure, comprising depositing a first isolation stack-nitride sublayer over a substrate at a first deposition rate; subsequently depositing a second isolation stack-nitride sublayer over said first isolation stack-nitride sublayer at a second deposition rate that is different from said first deposition rate; and further depositing a third isolation stack-nitride sublayer over said second isolation stack-nitride sublayer at a third deposition rate that is substantially equal to said first deposition rate.

  2. Claim 2Depends on #1

    The method as recited in claim 1 wherein said first isolation stack-nitride sublayer has a thickness that ranges from about 1 nm to about 40 nm.

  3. Claim 3Depends on #1

    The method as recited in claim 1 wherein said second isolation stack-nitride sublayer has a thickness that ranges

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Gary DePinto and Jim Wilson; "Optimization Of LPCVD Silicon Nitride Deposition Process by Use of Designed Experiments"; IEEE Advanced Semiconductor Manufacturing Conference; Sep. 11-12, 1990; pp. 47-53.
  • Gary DePinto and Jim Wilson; Optimization Of LPCVD Silicon Nitride Deposition Process by Use of Designed Experiments ; IEEE Advanced Semiconductor Manufacturing Conference; Sep. 11 12, 1990; pp. 47 53.
  • H. W. van Zeijl. L. K. Nanver and P.J. French; Low Stress Nitride as Oxidation Ask for Submicrometre LOCOS Isolation; IEEE Electron Device Letters; May 25, 1995; pp. 927 929.
  • H. W. van Zeijl. L. K. Nanver and P.J. French; Low-Stress Nitride as Oxidation Ask for Submicrometre LOCOS Isolation; IEEE Electron Device Letters; May 25, 1995; pp. 927-929.
  • H.W. van Zeijl, L.K. Nanver and P.J. French, "Low-stress nitride as oxidation mask for submicrometre LOCOS isolation", May 25, 1995-vol. 31-No. 11-Electronics Letters, (pp. 927).