Patents
US 6,090,171 A#13553465 Most CitedExpiredUnited States (USPTO)Utility

Stabilized thermally beneficiated low rank coal and method of manufacture

8Forward Citations (#13553465 Global)
0.3/yrCitation Velocity (#25117156 Global)
1.74Citation PageRank (#18105263 Global)
45Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process for reducing the spontaneous combustion tendencies of thermally beneficiated low rank coals employing heat, air or an oxygen containing gas followed by an optional moisture addition. Specific reaction conditions are supplied along with knowledge of equipment types that may be employed on a commercial scale to complete the process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 45 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    In a method for stabilizing and preventing the spontaneous combustion of particulate coal having pores and reactive sites, the improvement comprising heating the particulate coal with air of a temperature of 140°-350° F. and oxygenating said coal at a temperature of 140-250° F., for a process time of 30 minutes to 2 hours, then cooling said coal, and then repeating said heating and oxygenating, said alternate heating, cooling and reheating of the coal aiding in the diffusing of oxygen into the pores of said coal by forcing air to be drawn into the pores of the coal, thus allowing for a more co

  2. Claim 2Depends on #1

    The method of claim 1 wherein the coal is treated in a fluidized bed reactor wherein the air temperature is 200°-250° F., the coal temperature is 200-250 for a time period of 30 minutes to one hour.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (45)

PatentTitleYearCitations
GB 353,929 AA process for the calorific improvement of charcoal and other porous fuels—4
GB 636,033 AImprovements in or relating to oxidation of solid cabonaceous materials—5
US 2,966,400 ALignite processing method19609
GB 973,547 ARemoval of dust from combustible particles—3
US 3,723,079 AStabilization of coal197338
US 3,754,876 AUpgrading low rank coals as fuel197327
US 3,817,874 AProcess for increasing the surface area of active carbons197434
US 3,980,447 AProcess for the manufacture of brown coal briquettes197614
US 3,985,517 ACoal passivation process197666
US 4,053,285 AProcess for reducing the sulfide sulfur content of char with carbon dioxide and H2 O197718
US 4,170,456 AInhibiting spontaneous combustion of coal char197919
US 4,192,650 AProcess for drying and stabilizing coal198035
US 4,210,423 ASolid fuel use in small furnaces198058
US 4,249,909 ADrying and passivating wet coals and lignite198145
EP 0,081,763 A2Process for converting coal or mixtures thereof into a condition fit for the storage and transport thereof—4
US 4,396,395 AMethod and apparatus for contacting particulate coal and a deactivating fluid198316
US 4,396,394 AMethod for producing a dried coal fuel having a reduced tendency to spontaneously ignite from a low rank coal198343
US 4,400,176 AProcess for reducing the water content of coal containing bound water198315
US 4,401,436 AProcess for cooling particulate coal198338
US 4,402,706 AMethod and apparatus for oxidizing dried low rank coal198324
US 4,402,707 ADeactivating dried coal with a special oil composition198320
US 4,403,996 AMethod of processing low rank coal198314