Patents
US 6,087,440 A#2642735 Most CitedExpiredUnited States (USPTO)Utility

Continuous process for preparing a polyurethane latex

27Forward Citations (#2642735 Global)
1.0/yrCitation Velocity (#6122987 Global)
5.96Citation PageRank (#2492199 Global)
27Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A polyurethane/urea/thiourea latex having a narrow molecular weight polydispersity and sub-micron particle size can be prepared by first preparing a high solids (between about 65% and 74% solids) latex of a polyurethane/urea/thiourea prepolymer, then contacting the emulsion with a chain-extending reagent under such conditions to form the polymer latex.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 27.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a high solids content polyurethane/urea/thiourea latex comprising the steps of: a) continuously merging in the presence of an emulsifying and stabilizing amount of a surfactant a first stream containing water flowing at a rate r 1 , together with a second stream containing a polyurethane/urea/thiourea prepolymer flowing at a rate r 2 , to form a polyurethane/urea/thiourea latex prepolymer; and b) contacting the latex prepolymer with a chain-extending reagent under such conditions to form a polyurethane/urea/thiourea latex; wherein the ratio of r 2 :r 1 is not less t

  2. Claim 2Depends on #1

    The process of claim 1 wherein the polyurethane/urea/thiourea prepolymer is a polyurethane prepolymer or a polyurethane/urea prepolymer and wherein the p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 27 total)

PatentTitleYearCitations
CN 119,529,225 AHigh-performance room-temperature self-repairing polyurethane elastomer and preparation method thereof—0
US 7,435,787 B2Process for the continuous production of silylated resin200812
CN 107,082,860 ASelf-emulsifying waterborne polyurethane curing agent and preparation method thereof—16
WO 2008/077118 A3An ultra-high solid content polyurethane dispersion and a continuous process for producing ultra-high solid content polyurethane dispersions—0
US 12,031,054 B2Aqueous polyurethane dispersions for artificial leather applications20240
US 2003220463 A1Polyurethane dispersions—22
US 2007060735 A1Process for the continuous production of silylated resin—12
US 10,752,727 B1Process and apparatus for continuous production of aqueous polyurethane dispersions20200
US 8,821,983 B2Ultra-high solid content polyurethane dispersion and a continuous process for producing ultra-high solid content polyurethane dispersions20142
WO 2004/052956 A1Polyurethane prepolymer, stable aqueous dispersions with high solids containing the same and method of using and preparing the aqueous dispersions—16
US 2009312489 A1Device for producing dispersions and method of producing dispersions—5
US 2009054542 A1Eo/po block copolymers useful as stabilizers for pur foams—11
US 12,421,391 B2Polyether based waterborne polyurethane dispersion and method for preparing the same20250
US 2002177654 A1Process for preparing aqueous dispersions of hybrid polyurethane particles—33
US 2006111506 A1Filled polyurethane dispersions—2

Non-Patent Literature (2)

  • Hansen, C. M., J. Paint Technol., vol. 39, No. 511, pp. 505 510 (Aug. 1967).
  • Hansen, C. M., J. Paint Technol., vol. 39, No. 511, pp. 505-510 (Aug. 1967).