Abstract

This invention includes a semiconductor device having a gate formed on a semiconductor substrate with a low hydrogen content etch stop or barrier layer formed over the gate, and methods for manufacturing a semiconductor device with an etch stop or barrier layer with low free hydrogen content. The semiconductor device may have a hydrogen getter layer formed between the gate and the etch stop or barrier layer. The etch stop or barrier layer is a high temperature PECVD nitride film, a high temperature PECVD oxynitride film or a high temperature LPCVD nitride film. The hydrogen getter layer is P-doped film having a thickness between about 500 Å and about 2000 Å and is a PSG, BPSG, PTEOS deposited oxide film, or a BPTEOS deposited oxide film. The low free hydrogen content of the etch stop layer or barrier layer is achieved by a high temperature annealing step, performed at a higher temperature than the deposition temperature of the etch stop or barrier layer. Specific uses of the etch stop or barrier layers include manufacture of electrical contacts and local interconnects.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 53.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a semiconductor device on a semiconductor substrate, comprising: (a) forming, at a first temperature, one of an etch stop layer or a barrier layer overlying the semiconductor substrate; (b) annealing the layer formed in said step (a) at a second temperature higher than the first temperature to reduce the amount of free hydrogen in said layer; and (c) forming a cap layer overlying the layer formed in said steps (a) and (b) so that free hydrogen remains reduced in the layer formed in step (b).

  2. Claim 2Depends on #1

    The method of claim 1 wherein the step of forming one of the barrier layer and the etch stop layer further comprises forming a film selected from the group consisting of a high temperature PECVD nitride film, a high temperature PECVD oxynitride film and a high temperature LPCVD nitride film.

  3. Claim 3Independent Claim

    The

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Ghandhi, S. K., VLSI Fabrication Principles, Silicon and Gallium Arsenide, Second Edition, pp. 530 535, 728 730, 1994.
  • Ghandhi, S. K., VLSI Fabrication Principles, Silicon and Gallium Arsenide, Second Edition, pp. 530-535, 728-730, 1994.
  • Wolf, S., Silicon Processing for the VLSI Era, vol. 1 Process Technology, pp. 57, 58, 113 114 and 193 194, 1986.
  • Wolf, S., Silicon Processing for the VLSI Era, vol. 1--Process Technology, pp. 57, 58, 113-114 and 193-194, 1986.
  • Yoshida, S., Improvement of Endurance to Hot Carrier Degradation by Hydrogen Blocking P SiO, IEEE, IEDM, pp. 22 25, Dec. 11, 1988.