Patents
US 6,066,401 A#3184373 Most CitedExpiredUnited States (USPTO)Utility

Wide-band two-layer antireflection coating for optical surfaces

24Forward Citations (#3184373 Global)
0.9/yrCitation Velocity (#7724175 Global)
4.77Citation PageRank (#3576084 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process for forming a two-layer coating on glass or another substrate involves applying first a layer of light metal fluoride on the substrate and subsequently a layer of a porous metal oxide e.g. silica. The metal fluoride layer may be applied by using the sol-gel technique or by other methods e.g. vacuum deposition. The metal oxide layer is preferably applied by a sol-gel technique, by either a dip coating or spin coating. Each layer is preferably about one quarter-wavelength thick. The refractive index of the first layer is lower than that of the substrate, and the second layer has lower refractive index than the first layer. This dependence minimizes reflection of the coating over a broad wavelength range.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 24.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A two-layer antireflective coating on a substrate, comprising: a first layer of a light metal fluoride applied on the surface of the substrate, and a second layer of a porous metal oxide applied over the metal fluoride layer, the refractive index of said coating being substantially uniform throughout each of said layers and decreasing from said metal fluoride layer to said metal oxide layer.

  2. Claim 2Depends on #1

    The coating according to claim 1 wherein the refractive index of said first layer is lower than the refractive index of said substrate.

  3. Claim 3Depends on #1

    The coating according to claim 1 wherein the thickness of said first layer and said second layer is about one quarter-wavelength at a wavelength where a reflection minimum is desired.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 24 total)

PatentTitleYearCitations
US 6,383,629 B1Optical element having a water repellant coating constructed from a composite material of CaF2 and TiO220026
US 2004057142 A1Method of making stress-resistant anti-reflection multilayer coatings containing cerium oxide—6
US 11,609,363 B2Layered optical composite having a reduced content of highly refractive layers and its application in augmented reality20230
US 2005158591 A1Anti-reflection UV-blocking multilayer coatings having a thin film layer having cerium oxide, silicon dioxide and transition metal oxides—10
US 7,682,676 B2Optical element and optical pickup device20101
WO 0,158,681 A1Antireflective uv blocking multilayer coatings wherin film has cerium oxide—8
US 6,825,976 B2Antireflection coating for ultraviolet light20049
US 6,320,996 B1Wavelength selective optical switch2001104
US 2004028809 A1Porous layers and method for production thereof by means of spin-coating—37
US 12,242,057 B2Optical layered composite having two groupings of coating layers and its application in augmented reality20250
US 12,411,266 B2Optical layered composite having a reduced content of highly refractive layers and its application in augmented reality20250
US 2006166006 A1Article or transparent component having liquid repellent layer, optical lens having liquid repellent layer and production process thereof, and projection type display apparatus using the lens—2
CN 100,443,923 COptical system20080
US 8,883,935 B2High refractive index composition20144
US 7,435,482 B2Article or transparent component having liquid repellent layer, optical lens having liquid repellent layer and production process thereof, and projection type display apparatus using the lens20080