Patents
US 6,057,230 A#5275021 Most CitedExpiredUnited States (USPTO)Utility

Dry etching procedure and recipe for patterning of thin film copper layers

17Forward Citations (#5275021 Global)
0.7/yrCitation Velocity (#12179671 Global)
3.27Citation PageRank (#6583122 Global)
16Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for fabricating a copper, or a copper-titanium nitride-titanium, interconnect structure, using a low temperature RIE patterning procedure, has been developed. The RIE patterning procedure features the use of SiCl 4 and nitrogen, as reactants, with amount of nitrogen supplied, being equal to, or greater than, the SiCl 4 level. The addition of nitrogen, to the etching ambient, results in the formation of a non-cross-linked, by-product, which is easily removed during the patterning procedure, this not interfering with the creation of interconnect structure. Without the addition of nitrogen, a cross-linked, by-product, would be formed, during the low temperature RIE procedure, with the redeposited, cross-linked, by-product, interfering with the patterning of the copper interconnect structure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 17.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for forming a copper interconnect structure, on a semiconductor substrate, comprising the steps of: providing a insulator layer, on said semiconductor substrate, with openings in said insulator layer, exposing underlying conductive elements; depositing a copper layer on said insulator layer, and on said underlying conductive elements, exposed in the openings in said insulator layer; forming a photoresist shape, on said copper layer; patterning of said copper layer, using said photoresist shape as a mask, to form said copper interconnect structure, via a low temperature RIE proce

  2. Claim 2Depends on #1

    The method of claim 1, wherein said underlying conductive

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
US 5,447,599 ASelf-aligned process for capping copper lines199545
US 5,505,322 AProcess for etching copper containing metallic film and forming copper containing metallic wiring199610
US 5,539,256 ASemiconductor device having an interconnection of a laminate structure and a method for manufacturing the same199640
US 5,569,627 AProcess for etching copper containing metallic film and for forming copper containing metallic wiring19967
US 5,578,166 AMethod of reactive ion etching of a thin copper film199644
US 5,591,302 AProcess for etching copper containing metallic film and for forming copper containing metallic wiring199717
US 5,747,379 AMethod of fabricating seamless tungsten plug employing tungsten redeposition and etch back199863
US 5,792,672 APhotoresist strip method199836
US 5,866,947 APost tungsten etch bank anneal, to improve aluminum step coverage199919
US 5,930,669 AContinuous highly conductive metal wiring structures and method for fabricating the same1999260
US 5,960,317 AMethods of forming electrical interconnects on integrated circuit substrates using selective slurries199936
US 5,960,320 AMetal wiring layer forming method for semiconductor device199927
US 5,976,970 AMethod of making and laterally filling key hole structure for ultra fine pitch conductor lines199943
US 5,976,975 ARefractory metal capped low resistivity metal conductor lines and vias199950
US 5,976,972 AMethod of making semiconductor apparatus having wiring groove and contact hole formed in a self-alignment manner199938