Top-surface-metallurgy plate-up bonding and rewiring for multilayer devices

6Forward Citations (#18290987 Global)
0.2/yrCitation Velocity (#30812426 Global)
1.47Citation PageRank (#23658876 Global)
18Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A device repair process that includes removing a passivation polyimide layer. The passivation polyimide layer is removed using a first-half ash followed by a second-half ash. The device is rotated during the second-half ash. The device is then cleaned using sodium hydroxide (NaOH) and a subsequent light ash step is implemented. After the passivation polyimide layer is removed, a seed layer is deposited on the device. A photoresist is formed on the seed layer and bond sites are formed in the photoresist. Repair metallurgy is plated through the bond sites. The bond sites are plated by coupling the device to a fixture and applying the current for plating to the fixture. The contact between the device and the fixture is made though bottom surface metallurgy. After plating, the residual seed layer is removed and a laser delete process is implemented to disconnect and isolate the nets of the device.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process of repairing a device having wiring nets, the process comprising the steps of: (a) depositing a sputtered seed layer on the device; (b) forming a photoresist having bond sites; (c) plating repair metallurgy through the bond sites; and (d) conducting a laser delete process to disconnect and isolate at least one of the wiring nets of the device.

  2. Claim 2Depends on #1

    The process according to claim 1 wherein the process further comprises the step of (e) removing a layer.

  3. Claim 3Depends on #2

    The process according to claim 2 wherein step (e) further comprises the steps of: (e1) performing a first-half ash; (e2) performing a second-half ash; (e3) cleaning the device; and (e4) performing a further ash.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

Non-Patent Literature (5)

  • "Laser Deposition of Metal Films With Organo-Metal Ink", IBM Technical Disclosure Bulletin, vol. 31, No. 7, Dec. 1988, pp. 45-46.
  • "Localized Laser Deposition of Gold From Solid Salts", Research Disclosure, Kenneth Mason Publications Ltd., England, No. 293, Sep. 1988.
  • F.M. Tappen, "Open Conductor Repair For Glass Metal Module", IBM Technical Disclosure Bulletin, vol. 14, No. 10, Mar. 1972, p. 2915.
  • F.M. Tappen, Open Conductor Repair For Glass Metal Module , IBM Technical Disclosure Bulletin, vol. 14, No. 10, Mar. 1972, p. 2915.
  • Laser Deposition of Metal Films With Organo Metal Ink , IBM Technical Disclosure Bulletin, vol. 31, No. 7, Dec. 1988, pp. 45 46.