Patents
US 6,038,882 A#4608247 Most CitedExpiredUnited States (USPTO)Utility

Absorption chiller-heater and method for forming initial anticorrosive film therefor

19Forward Citations (#4608247 Global)
0.7/yrCitation Velocity (#10397985 Global)
2.79Citation PageRank (#8539708 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An object of the present invention is to provide a method for forming an initial anticorrosive film in an absorption chiller-heater, by selecting optimal conditions of absorbent solution, steel material surface and film-forming operation for forming a good initial anticorrosive film. In the process for forming an initial anticorrosion film in an absorption chiller-heater having steel parts and containing an absorbent solution comprising lithium bromide as its main component and containing a lithium molybdate corrosion inhibitor according to the present invention, the main characteristics are that at least part of the steel parts of the absorption chiller-heater contacting with an absorbent solution at a temperature of higher than 100° C. include a bare metal surface having an arithmetic mean surface roughness of not more than 1.0 μm; the absorbent solution supplied comprises lithium bromide as its main component and contains a lithium molybdate corrosion inhibitor dissolved in the solution at a level of 450-750 ppm; and that an initial anticorrosion film forming operation is conducted at a condition such that amount of the lithium molybdate dissolved in the absorbent solution is ma

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An absorption chiller-heater having steel parts and containing an absorbent solution comprising lithium bromide as its main component and containing a lithium molybdate corrosion inhibitor, wherein at least part of the steel parts contacting with the absorbent solution include a bare metal surface having an arithmetic mean surface roughness of not more than 1.0 μm, which surface has then been coated with lithium molybdate whereby a lithium molybdate film having high anticorrosive power is formed on the surface.

  2. Claim 2Depends on #1

    The absorption chiller-heater according to claim 1, wherein the steel parts contacting with the absorbent solution constitute at least one of a high-temperature regenerator, low-temperature regenerator or high-temperature heat exchanger.

  3. Claim 3Depends on #1

    The absorption chiller-heater according to claim 1, wherein th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗