Abstract
Expandable bladders for use in curing presses for hydrocarbon rubbers, such as pneumatic tires, are a crosslinked elastomer composition including isobutylene repeat units. When PTFE and/or graphite is present, they can be cured with brominated phenolic resins in shorter periods of time. The fluorinated ethylene polymer is added in particulate form and thereafter dispersed throughout the bladder. The fluorinated ethylene polymer may or may not form fibers. The bladders may further include graphite. The bladders generally have enhanced lubricity, reduced adhesion to cured tire innerliners, better resistance to cracking during flexing, and have lower tension set than similar compositions without fluorinated ethylene polymers. The above enhancements allow hydrocarbon rubbers such as tires to be molded with fewer defects caused by abraded or deformed bladders. They also enhance the useful life of the bladder reducing the cost of tire curing.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 21.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In a curing press for a hydrocarbon rubber composition which uses an expandable bladder to assist in shaping and curing said rubber composition; the improvement wherein the bladder comprises crosslinks derived from about 0.5 to about 12 parts by weight of a halogenated phenolic resin curative and either from about 0.5 to about 10 parts by weight of at least one fluorinated ethylene polymer; or from about 0.1 to about 20 parts by weight of graphite; molybdenum disulfide and/or tungsten disulfide or combinations thereof, and wherein said fluorinated ethylene polymer and/or said graphite, molybde
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 21 total)
References Cited — Backward Prior Art (18)
Non-Patent Literature (5)
- "Standard Test Methods for Vulcanized Rubber and Thermoplastic Rubbers and Thermoplastic Elastomers-Tension1 ", published by ASTM; Philadelphia, PA, Nov. 15, 1992 ASTM D412-92.
- Chapter 10 of Rubber Technology 2 nd Ed., Edited by Maurice Morton, published by Robert E. Krieger Publishing Co.: Malabar, Florida, Jan. 1, 1973, pp. 249 273.
- Chapter 10 of Rubber Technology 2nd Ed., Edited by Maurice Morton, published by Robert E. Krieger Publishing Co.: Malabar, Florida, Jan. 1, 1973, pp. 249-273.
- Standard Test Methods for Vulcanized Rubber and Thermoplastic Rubbers and Thermoplastic Elastomers Tension 1 , published by ASTM; Philadelphia, PA, Nov. 15, 1992 ASTM D412 92.
- Technical Data Sheets SP1055 Flaked Resin from Schenectady International in Schenectady New York released on Oct. 9, 1996 (2 pages).