A high temperature superconductor composite material, which is suitable for production of filaments, wires, coils and other shaped products, has a ceramic powder of a material selected from the group consisting of, for example, YBa 2 Cu 3 O 7-x and Bi 2 Sr 2 Ca 2 Cu 3 O 10 ; a solution of a material selected from the group consisting of rubber silicone or lacquer silicone in a substance selected from the group consisting of toluene or acetone; and an ultra-fine silver powder dope, and is produced by using an emulsion mixture of the three major components with ultrasonic homogenization of the mixture, primer cladding of a glue-exterior layer on a silver core filament, high temperature superconductor coating of the silver core by chemical adhesion, and polymerization of the coating applied by low temperature heating, whereafter the composition is treated by magnetic treatment, gamma irradiation, and microwave supported fast heating.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 13.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of production a high temperature superconductor product from composite, comprising the steps of making an emulsion mixture of a superconductor ceramic powder, silicone material selected from the group consisting of rubber silicone and lacquer silicone, and an ultra-fine silver powder dope; forming a product from the emulsion; treating the formed product by a process selected from the group consisting of a chemical process, a physical process and a thermal process; and sintering the product.

  2. Claim 2Depends on #1

    A method as defined in claim 1, wherein the rubber silicone or lacquer silicone have a molecular weight within the range of 20,000-800,000 and is present in the material in the mass ratio 2%-8%.

  3. Claim 3Depends on #1

    A method as defined in claim 1,